Assessment of Strength and Bending of Concrete Containing Crushed Glass and Fibers

Assessment of Strength and Bending of Concrete Containing Crushed Glass and Fibers

Authors

  • Ali Akbar Firoozi

    Department of Civil Engineering, Faculty of Engineering & Technology, University of Botswana, Gaborone, Botswana.

  • Ali Asghar Firoozi

    Department of Civil Engineering, Faculty of Engineering & Technology, University of Botswana, Gaborone, Botswana.

  • Mahongo Dithinde

    Department of Civil Engineering, Faculty of Engineering & Technology, University of Botswana, Gaborone, Botswana.

  • Obakeng Bome

    Department of Civil Engineering, Faculty of Engineering & Technology, University of Botswana, Gaborone, Botswana.

DOI:

https://doi.org/10.55121/nefm.v3i1.55

Keywords:

Concrete, Compressive strength, Flexural test, PET fibres, Crushed waste glass

Abstract

Abstract

This paper presents proposed investigations of the influence of crushed glass and fibers on the mechanical properties of concrete. Conventional concrete has lack tension in order to improve its flexural strength and compressive strength. This study has adopted the addition of PET fibers and recycled waste glass fibers to concrete. The study uses M25 grade concrete to study the effects of adding crushed waste glass at a weight of 0, 5, 10, and 15%. The PET fibers were extracted from waste bottles used for packaging of drinks and hand cut into very small rectangular pieces (with an average size of 3×10mm). For the mix design, the addition of 0, 3, 5, and 10% dosages of PET fiber was adopted to compare their influence against plain concrete with no fiber addition. Both fiber samples were tested for compressive strength and flexural strength and samples were cured for 7, 28, 56, and 90 days. Results showed that the combination of using crushed glass and PET fibers has a significant effect on compressive strength (i.e., 122%) and flexural beam test (56%) for 90 days of cured samples.

References

[1] Yermak, N., Pliya, P., Simon, A., & Noumowe, A. (2017). Influence of steel and/or polypropylene fibres on the behaviour of concrete at high temperature: Spalling, transfer and mechanical properties. Construction and Building Materials, 240-250.

[2] Pliya Prosper, B. A.-L. (2009). Strength and porosity of concrete incorporating polypropylene and steel fibres subjected to high temperatures. 20th International Conference on Structural Mechanics in Reactor Technology (SMiRT 20), 9-14.

[3] Feng Shi, T. M. (2022). Post-cracking behaviour of basalt and macro polypropylene hybrid fibre reinforced concrete with different compressive strength. Construction and Building Materials, 262-275.

[4] Pietro Lura, O. M. (2009). Cracking in cement paste induced by autogenous shrinkage. Materials and Structures, 1089-1099.

[5] Szeląg, M. (2019). Evaluation of cracking patterns of cement paste containing polypropylene fibres. Composite Structures, 402-411.

[6] Vikrant S. Vairagade, K. S. (2013). Strength of Normal Concrete Using Metallic and Synthetic Fibers. Chemical, Civil and Mechanical Engineering Tracks of 3rd Nirma University International Conference, 132-140.

[7] Fraternali, F., Ciancia, V., Chechile, R., Rizzano, G., Feo, L., & Incarnato, L. (2011). Experimental study of the thermo-mechanical properties of recycled PET fiber-reinforced concrete. Composite structures, 93(9), 2368-2374.

[8] Jansson, A., Flansbjer, M., Löfgren, I., Lundgren, K., & Gylltoft, K. (2012). Experimental investigation of surface crack initiation, propagation and tension stiffening in self-compacting steel–fibre-reinforced concrete. Materials and structures, 45(8), 1127-1143.

[9] FRCA (2007). Applications and Fiber Types. Retrieved September 2013, from Fiber-Reinforced Concrete Association - FRCA

[10] Zainab Z. Ismail, E. A.-H. (2009). Recycling of waste glass as a partial replacement for fine aggregate in concrete. Waste Management, 655–659.

[11] Gautam, S. P., Srivastava, V., & Agarwal, V. C. (2012). Use of glass wastes as fine aggregate in Concrete. J. Acad. Indus. Res, 1(6), 320-322.

[12] Mardani-Aghabaglou, A., Tuyan, M., & Ramyar, K. (2015). Mechanical and durability performance of concrete incorporating fine recycled concrete and glass aggregates. Materials and Structures, 48(8), 2629-2640.

[13] Rahmani, E., Dehestani, M., Beygi, M. H. A., Allahyari, H., & Nikbin, I. M. (2013). On the mechanical properties of concrete containing waste PET particles. Construction and Building Materials, 47, 1302-1308.

[14] Ajamu, S. O., Ige, J. A., & Oyinkanola, T. M. Effect of Waste (PET) Bottle Fibers on The Properties of Concrete. International Journal of Research of Engineering and Technology, 6, 1-8.

[15] S.S. Asadi, S. P. (2021). An experimental crack evolution of concrete with fly-ash and hybrid fibers. Materials Today: Proceedings, 2083-2090.

[16] Ramesh, K., Arunachalam, K., and Chakravarthy, R. S. (2013). Experimental investigation on impact resistance of fly ash concrete and fly ash fibre reinforced concrete. IJERA. vol. 3, Issue 2, pp. 990-999, ISSN: 2248-9622.

[17] Irvan, S. (1996). Mechanical properties of high performance concrete. ACI Mater. J., 93(5), 416-426.

[18] Walis, S. (1995). Steel fibre developments in South Africa, Tunnels and Tunnelling, issue 3, pp. 22-24.

Downloads

Published

2024-03-12

How to Cite

Firoozi, A. A., Firoozi, A. A., Dithinde, M., & Bome, O. (2024). Assessment of Strength and Bending of Concrete Containing Crushed Glass and Fibers. New Environmentally-Friendly Materials, 3(1), 1–11. https://doi.org/10.55121/nefm.v3i1.55

Issue

Section

Articles
Loading...